Teflon Veton Rings

Teflon Veton Rings

Home Forums General Questions Teflon Veton Rings

Viewing 5 posts - 1 through 5 (of 5 total)
  • Author
    Posts
  • #333937
    BOB BLACKSHAW 1
    Participant
      @bobblackshaw1

      I am nearly finished making the Potty mill engine but the drawing calls for Teflon or Veton ring for the piston and two other for making a seal. I have made several Beam engines running on air with out rings just a small grove in the piston for oil and have had them running on very low pressure. I don't intend to run the mill engine on steam but would like to know where I can get these rings.Ive looked on the internet but cant find what I need,

      #25719
      BOB BLACKSHAW 1
      Participant
        @bobblackshaw1
        #333939
        John Olsen
        Participant
          @johnolsen79199

          Teflon rings are mostly home made from teflon rod as far as I know. Viton (not Veton) rings are O rings, you should be get them from good engineering supply firms. If you are not running steam at high temperatures, ordinary nitrile O rings would be fine.

          John

          #333949
          JasonB
          Moderator
            @jasonb

            As Stew uses metric sizes you will have to get metric rings to suit, I have used these people a few times who have a good range of the Vitron ones.

            You can also fill the ring groove with Graphite or PTFE inpregnated yarn which is less critical on the correct groove size. This can also be used as gland packing.

            If you are just running for display then you should be able to get away with no rings if fit and finish is reasonable, this will also have less sticktion so better for slow running.

            Edited By JasonB on 26/12/2017 07:08:18

            #333986
            Jon
            Participant
              @jon

              Another for Sealforce, 8/10 next day delivery, quality seals and measure whats sold, many dont. Local hydraulics may want a minimum charge and order.

              Generally Viton starts at 75 shore against Nitrile 70 shore and lasts hell of a lot longer.

              Viton® temperature rating

              Depending on the grade the working temperature range is considered to be -26°C to +205°/230°C (-15°F to +400°/440°F). But for short working periods it will take even higher temperatures.

            Viewing 5 posts - 1 through 5 (of 5 total)
            • Please log in to reply to this topic. Registering is free and easy using the links on the menu at the top of this page.

            Latest Replies

            Home Forums General Questions Topics

            Viewing 25 topics - 1 through 25 (of 25 total)
            Viewing 25 topics - 1 through 25 (of 25 total)

            View full reply list.